MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing electrical insulation and shock resistance.

Key Features:

  • Convenient 10:1 mixing ratio for use in automatic dispensing equipment or hand mixing
  • Contains no solvents
  • Non-yellowing catalyst system
  • Chemical composition provides hydrolytic stability and reversion resistance
Part of the Amber Chemical Group. Data provided by manufacturer

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccQSil 216B
 1.02 g/cc1.02 g/ccQSil 216A
Viscosity 500 cP500 cPQSil 216B
 4000 cP4000 cPQSil 216A
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/incured 60 mins @ 100°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040cured 60 mins @ 100°C
Tensile Strength 5.20 MPa754 psicured 60 mins @ 100°C
Elongation at Break 100 %100 %cured 60 mins @ 100°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+15 ohm-cm1.70e+15 ohm-cm
Dielectric Constant 2.69
@Frequency 1000 Hz
2.69
@Frequency 1000 Hz
Dielectric Strength 19.7 kV/mm500 kV/in
Dissipation Factor 0.00060
@Frequency 1000 Hz
0.00060
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 275 µm/m-°C
@Temperature 20.0 °C
153 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.26 J/g-°C0.301 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4061.406cured 60 mins @ 100°C
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Gel Time 96.0 min96.0 min
 
Descriptive Properties
ColorClearQSil 216A
 ClearQSil 216B
 Transparent, colorlessCatalyzed
ConsistencyEasily pourable Catalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet)
CHT Group QSil 553 QSI Quantum Silicones Silicone Potting Material
Abatron L060421-1 Heat-Resistant Non-Flammable Silicone Rubber
CHT Group QGel 300 QSI Quantum Silicones High Strength Gel
CHT Group QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material

PACC036 / 22163

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.