MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Medium Density Polyethylene (MDPE), Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.928 - 0.950 g/cc0.0335 - 0.0343 lb/in³Average value: 0.938 g/cc Grade Count:36
Water Absorption 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:4
Environmental Stress Crack Resistance 30.0 - 5000 hour30.0 - 5000 hourAverage value: 1070 hour Grade Count:8
 19.0 - 220 hour
@Temperature 30.0 - 50.0 °C
19.0 - 220 hour
@Temperature 86.0 - 122 °F
Average value: 876 hour Grade Count:16
Melt Flow 0.0900 - 85.0 g/10 min0.0900 - 85.0 g/10 minAverage value: 9.74 g/10 min Grade Count:36
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 59.0 - 63.059.0 - 63.0Average value: 61.4 Grade Count:9
Tensile Strength, Ultimate 9.20 - 33.0 MPa1330 - 4790 psiAverage value: 18.9 MPa Grade Count:13
Tensile Strength, Yield 14.0 - 24.1 MPa2030 - 3500 psiAverage value: 19.5 MPa Grade Count:24
Elongation at Break 16.0 - 1210 %16.0 - 1210 %Average value: 463 % Grade Count:18
Elongation at Yield 8.00 - 13.0 %8.00 - 13.0 %Average value: 10.9 % Grade Count:10
Modulus of Elasticity 0.350 - 0.840 GPa50.8 - 122 ksiAverage value: 0.648 GPa Grade Count:7
Flexural Modulus 0.480 - 0.970 GPa69.6 - 141 ksiAverage value: 0.769 GPa Grade Count:27
Izod Impact, Notched 1.44 - 5.60 J/cm2.70 - 10.5 ft-lb/inAverage value: 3.77 J/cm Grade Count:3
Charpy Impact, Notched 0.800 - 0.800 J/cm²
@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.800 J/cm² Grade Count:1
Tensile Impact Strength 130 - 353 kJ/m²61.9 - 168 ft-lb/in²Average value: 221 kJ/m² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmAverage value: 1.00e+15 ohm-cm Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 - 500 µm/m-°C
@Temperature -20.0 - 100 °C
50.0 - 278 µin/in-°F
@Temperature -4.00 - 212 °F
Average value: 295 µm/m-°C Grade Count:1
Melting Point 117 - 131 °C243 - 268 °FAverage value: 126 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 47.0 - 77.8 °C117 - 172 °FAverage value: 54.7 °C Grade Count:19
Deflection Temperature at 1.8 MPa (264 psi) 37.3 - 41.0 °C99.1 - 106 °FAverage value: 38.5 °C Grade Count:17
Vicat Softening Point 62.0 - 124 °C144 - 255 °FAverage value: 104 °C Grade Count:14
Brittleness Temperature -118 - -70.0 °C-180 - -94.0 °FAverage value: -90.6 °C Grade Count:5
Flammability, UL94 HBHBGrade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 220 °C320 - 428 °FAverage value: 198 °C Grade Count:5
Melt Temperature 170 - 315 °C338 - 599 °FAverage value: 231 °C Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Poly-L-lactide (PLLA)
Overview of materials for Medium Density Polyethylene (MDPE), Extruded

O3900 / 78268

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.