MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Toyobo Fortron® FX72T6 PPS, Impact Modified
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: Product Description: Forton FX72T6 is an unreinforced, impact modified PPS with high flowability and high impact resistance suitable for injection molding. The mechanical properties reported on this data sheet refer to a mold wall temperature of 135°C.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Additive: Impact Modifier

Features: Impact Modified

Uses: Automotive Applications

Automotive Specifications: FORD WSS-M4D1063-A2

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inISO 294-4
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 310 °C
35 g/10 min
@Load 4.76 lb,
Temperature 590 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiISO 527-2/5
Elongation at Break 20 %20 %ISO 527-2/5
Tensile Modulus 1.68 GPa244 ksiISO 527-1
Flexural Modulus 1.70 GPa247 ksiISO 178
Poissons Ratio 0.410.41ISO 527
Izod Impact, Notched (ISO) 10.1 kJ/m²4.80 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) NBNBISO 180/1U
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 1.01 J/cm²4.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.00030
@Frequency 1e+6 Hz
0.00030
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  86.4 µm/m-°C
@Temperature -30.0 - 70.0 °C
48.0 µin/in-°F
@Temperature -22.0 - 158 °F
ISO 11359-2
 130 µm/m-°C
@Temperature 110 - 200 °C
72.0 µin/in-°F
@Temperature 230 - 392 °F
ISO 11359-2
CTE, linear, Transverse to Flow  97.2 µm/m-°C
@Temperature 70.0 - 110 °C
54.0 µin/in-°F
@Temperature 158 - 230 °F
ISO 11359-2
 140 µm/m-°C
@Temperature 110 - 200 °C
78.0 µin/in-°F
@Temperature 230 - 392 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FUnannealed; ISO 75-2/A
Vicat Softening Point 122 °C252 °FISO 306/B50
Flammability, UL94 V-0
@Thickness 3.05 mm
V-0
@Thickness 0.120 in
Oxygen Index 49 %49 %ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °FHopper
 290 - 320 °C554 - 608 °FHot Runner
Feed Temperature 60.0 - 75.0 °C140 - 167 °FInjection
Rear Barrel Temperature 280 - 300 °C536 - 572 °F
Middle Barrel Temperature 285 - 305 °C545 - 581 °F
Front Barrel Temperature 285 - 305 °C545 - 581 °F
Nozzle Temperature 290 - 320 °C554 - 608 °F
Zone 4 290 - 310 °C554 - 590 °FInjection
Melt Temperature 290 - 320 °C554 - 608 °F
Mold Temperature 50.0 - 135 °C122 - 275 °F
Drying Temperature 100 °C212 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Back Pressure <= 3.50 MPa<= 508 psi
Screw Speed  50 rpm
@Thickness 55.9 mm
50 rpm
@Thickness 2.20 in
 75 rpm
@Thickness 40.6 mm
75 rpm
@Thickness 1.60 in
 120 rpm
@Thickness 24.9 mm
120 rpm
@Thickness 0.980 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6289 / 310982

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.