MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Torlon® 4275 PAI, Good wear resistance at high velocities
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Graphite Filled

Material Notes: Good wear resistance at high velocities, contains PTFE and graphite

Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with a low coefficient of friction and outstanding wear resistance at both high velocity and high pressure conditions.

Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep and chemicals.

Potential applications for Torlon® 4275 polyamide-imide include thrust washers, spline liners, valve seats, bushings, bearings, wear rings, cams and other applications requiring strength at high temperature and resistance to wear.

Applications: Aerospace Applications; Aircraft Applications; Automotive Applications; Bearings; Bushings; Gears; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Rollers; Sealing Devices; Seals; Thrust Washer; Transmission Applications; Washer

Features: Chemical Resistant; Creep Resistant; Flame Retardant; High Heat Resistance; High Temperature Strength; Low Friction; Self Lubricating; Semi Conductive; Wear Resistant

Injection notes: Minimum drying conditions: 3 hours at 350°F (177°C), 4 hours at 300°F (149°C), or 16 hours at 250°F (121°C).
Compression Ratio: 1:1 to 1.5:1
Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence.
Molded parts must be post cured.

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.33 %
@Time 86400 sec
0.33 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 - 0.0045 cm/cm0.0025 - 0.0045 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 117 MPa17000 psiASTM D638
Tensile Stress 131 MPa19000 psiASTM D1708
Tensile Modulus 7.79 GPa1130 ksiASTM D638
 8.83 GPa1280 ksiASTM D638
Flexural Strength  110 MPa
@Temperature 232 °C
16000 psi
@Temperature 450 °F
ASTM D790
 208 MPa
@Temperature 23.0 °C
30200 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus  5.10 GPa
@Temperature 232 °C
740 ksi
@Temperature 450 °F
ASTM D790
 7.31 GPa
@Temperature 23.0 °C
1060 ksi
@Temperature 73.4 °F
ASTM D790
Compressive Strength 123 MPa17800 psiASTM D695
Compressive Modulus 4.00 GPa580 ksiASTM D695
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM D256
Izod Impact, Unnotched 2.70 J/cm5.06 ft-lb/inASTM D256
Coefficient of Friction 0.050 - 0.310.050 - 0.31ASTM D1894
K (wear) Factor  1.40 x 10-8 mm³/N-M
@Pressure 5.20 MPa
0.695 x 10-10 in³-min/ft-lb-hr
@Pressure 754 psi
0.38 m/sec; ASTM D3702
 26.0 x 10-8 mm³/N-M
@Pressure 3.40 MPa
12.9 x 10-10 in³-min/ft-lb-hr
@Pressure 493 psi
0.25 m/sec; ASTM D3702
 26.0 x 10-8 mm³/N-M
@Pressure 3.40 MPa
12.9 x 10-10 in³-min/ft-lb-hr
@Pressure 493 psi
0.25 m/sec; ASTM D3702
 35.0 x 10-8 mm³/N-M
@Pressure 0.220 MPa
17.4 x 10-10 in³-min/ft-lb-hr
@Pressure 31.9 psi
4.1 m/sec; ASTM D3702
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+15 ohm-cm8.00e+15 ohm-cmASTM D257
Surface Resistance 4.00e+17 ohm4.00e+17 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C13.9 µin/in-°FASTM D696
Thermal Conductivity 0.650 W/m-K4.51 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 304 °C579 °F
Nozzle Temperature 371 °C700 °F
Mold Temperature 199 - 216 °C390 - 421 °F
Drying Temperature 177 °C
@Time 10800 sec
351 °F
@Time 3.00 hour
Moisture Content <= 0.050 %<= 0.050 %Injection
Back Pressure 6.89 MPa999 psi
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AdditivePTFE + Graphite Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw L/D Ratio, Injection18.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4546 / 280346

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.