MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 2311 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide improved pourability characteristics for cold powder compression molding. UL recognized under component file E40654. 02311 is available in black or brown color.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 g/cc0.0231 lb/in³ASTM D1895
Density 1.41 g/cc0.0509 lb/in³ASTM D792
Water Absorption 0.43 %0.43 %ASTM D570
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8383ASTM D785
Tensile Strength, Ultimate 59.0 MPa8560 psiASTM D638
Elongation at Break 0.86 %0.86 %ASTM D638
Tensile Modulus 8.20 GPa1190 ksiASTM D638
Flexural Strength 86.0 MPa12500 psiASTM D790
Flexural Modulus 7.30 GPa1060 ksiASTM D790
Compressive Strength 198 MPa28700 psiASTM D695
Poissons Ratio 0.330.33ASTM D638
Shear Modulus 3.08 GPa447 ksiCalculated
Izod Impact, Notched 0.163 J/cm0.305 ft-lb/inASTM D256
Charpy Impact, Notched 0.178 J/cm²0.847 ft-lb/in²ASTM D256
Impact 9898J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.20e+11 ohm-cm2.20e+11 ohm-cmASTM D247
Dielectric Constant 5.25.2ASTM D150
Dielectric Strength 9.30 kV/mm236 kV/inShort Time; ASTM D149
Dissipation Factor 0.0830.083ASTM D150
Arc Resistance 144 sec144 secASTM D495
Comparative Tracking Index 150 V150 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 57.0 µm/m-°C
@Temperature 40.0 - 130 °C
31.7 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.400 W/m-K
@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 201 °C394 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 157 °C315 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 27 %27 %ASTM D2863
Shrinkage 0.42 %0.42 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1581 Polyester, Pellet, Injection Molded
Plenco 2311 Phenolic, Granular, Transfer Molded
Plenco 2311 Phenolic, Granular, Compression Molded
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1500 Polyester, Granular, Transfer Molded

PLEL39 / 50607

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.