MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Indium Corp. Indalloy® 131 97Sn/3Sb Lead-Free Solder Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: Information provided by the manufacturer, Indium Corporation.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.26 g/cc0.262 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 9.65 MPa1400 psi
 
Thermal PropertiesMetricEnglishComments
Melting Point 232 - 238 °C450 - 460 °F
Solidus 232 °C450 °F
Liquidus 238 °C460 °F
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb 3.0 %3.0 %
Tin, Sn 97 %97 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy
Indium Corp. Indalloy® 129 99Sn/1Sb Lead-Free Solder Alloy
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy
Indium Corp. Indalloy® 1E In-Sn Solder Alloy
Indium Corp. Indalloy® 201 Sn-Zn Solder Alloy

NNIN63 / 18515

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.