MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

INEOS Styrolution Terlux® 2802 Transparent MABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Terlux® 2802 is a standard injection molding grade based on a MABS polymer. Terlux® 2802 offers an unique combination of properties, such as a balanced stiffness/toughness ratio and the high transparency well known in SAN molding compositions. Excellent transparency, Good resistance to chemicals, Good stiffness and surface finish, High impact strength.

Applications: Cosmetic packaging, Housewares, Housings, Toys, sport and leisure.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.590 g/cc0.0213 lb/in³with external lubricant
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Water Absorption at Saturation 0.70 %
@Temperature 23.0 °C
0.70 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow  2.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
2.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 17 g/10 min
@Load 21.6 kg,
Temperature 220 °C
17 g/10 min
@Load 47.6 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 70.0 MPa10200 psiISO 2039-1
Tensile Strength, Yield 48.0 MPa6960 psiISO 527
Elongation at Break 12 %12 %Nominal; ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Flexural Strength 70.0 MPa10200 psiISO 178
Izod Impact, Notched 0.690 J/cm
@Thickness 3.17 mm
1.29 ft-lb/in
@Thickness 0.125 in
ASTM Test
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 1250 MPa181000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
IEC 60250
 0.016
@Frequency 100 Hz
0.016
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  93.0 °C
@Load 5.10 kg
199 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 105 °C
@Load 1.02 kg
221 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54Sodium D Line; ISO 489
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °FISO 294
Mold Temperature 50.0 - 75.0 °C122 - 167 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
Drying Temperature 70.0 °C
@Time 7200 sec
158 °F
@Time 2.00 hour
 
Compliance PropertiesMetricEnglishComments
NSF NoNoNSF Std. 51
 NoNoNSF Std. 61
 
Descriptive Properties
ColorClear
Commercial StatusNorth America and Europe
Impact ModifiedYes
Injection Molding Regrind<10%
Primary Processing TechniqueInjection Molding
ProcessingBlow Molding
 Film Extrusion
 Injection Molding
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
Special characteristicPlatable
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terlux® HD 2802 MABS
INEOS Styrolution Terlux® 2812 Transparent MABS
INEOS Styrolution Terlux® 2802 TR Q434 Transparent MABS
Chi Mei Polylac® PA-758 ABS - Transparent
Ineos ABS Lustran® 266 ABS, Transparent Grade

PBASF9054 / 84818

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.