MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 4207 Thermoplastic Polyimide (TPI), Glass Fiber - UL94 V-0
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Glass Fiber

Material Notes: Properties are based on annealled specimens.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/ccASTM D 792
Filler Content 40 %40 %Primary Additive
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 124124ASTM D 785
Tensile Strength at Break 193 MPa28000 psiASTM D 638
Elongation at Break 2.0 %2.0 %ASTM D 638
Tensile Modulus 13.8 GPa2000 ksiASTM D 638
Flexural Strength 296 MPa43000 psiASTM D 790
Flexural Modulus 13.1 GPa1900 ksiASTM D 790
Izod Impact, Notched 1.44 J/cm
@Thickness 3.17 mm
2.70 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 10.7 J/cm
@Thickness 3.17 mm
20.0 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 316 °C>= 600 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 399 - 416 °C750 - 780 °F
Mold Temperature 177 - 232 °C350 - 450 °F
Drying Temperature 204 °C400 °F
Dry Time 6 hour6 hour
Moisture Content 0.010 %0.010 %
Dew Point -40.0 °C-40.0 °F
Injection Pressure 138 - 193 MPa20000 - 28000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 40% Glass Fiber Filled
RTP Company RTP 4287 Thermoplastic Polyimide (TPI), Carbon Fiber
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced

PQZWA2362 / 91111

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.