MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Die Cast
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Used in bearing applications. ZA-12 has a higher bearing load capacity than bronze bearing alloys, although its environment (both temperature and corrosive) is more limited.

Key Words: UNS Z35630 (ingot); UNS Z35631 (Casting); ZA-12 Zinc Foundry Alloy; Previously ILZRO 12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.04 g/cc0.218 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 100100500 kg load; 10 mm hardened steel ball
Hardness, Knoop 125125Estimated from Brinell Value
Hardness, Rockwell A 41.541.5Estimated from Brinell Value
Hardness, Rockwell B 6363Estimated from Brinell Value
Hardness, Vickers 112112Estimated from Brinell Value
Tensile Strength, Ultimate 404 MPa58600 psi
Tensile Strength, Yield 320 MPa
@Strain 0.2 %
46400 psi
@Strain 0.2 %
Elongation at Break 5.0 %5.0 %in 5 cm
Modulus of Elasticity 83.0 GPa12000 ksi
Compressive Strength 269 MPa39000 psi
Fatigue Strength 117 MPa
@# of Cycles 5.00e+8
17000 psi
@# of Cycles 5.00e+8
Reverse Bend
Fracture Toughness 14.4 MPa-m½13.1 ksi-in½
Shear Strength 296 MPa42900 psi
Charpy Impact, Unnotched 12.0 J
@Thickness 6.35 mm
8.85 ft-lb
@Thickness 0.250 in
square bar
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000610 ohm-cm0.00000610 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 118 J/g50.8 BTU/lb
CTE, linear 24.1 µm/m-°C
@Temperature 20.0 °C
13.4 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.450 J/g-°C
@Temperature 20.0 - 100 °C
0.108 BTU/lb-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 116 W/m-K805 BTU-in/hr-ft²-°F
Melting Point 377 - 432 °C711 - 810 °F
Solidus 377 °C711 °F
Liquidus 432 °C810 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 460 - 490 °C860 - 914 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10.5 - 11.5 %10.5 - 11.5 %Addition, Casting
 10.8 - 11.5 %10.8 - 11.5 %Addition, Ingot form
Cadmium, Cd <= 0.0050 %<= 0.0050 %Impurity, Ingot form
 <= 0.0060 %<= 0.0060 %Impurity, Casting
Copper, Cu 0.50 - 1.2 %0.50 - 1.2 %Addition, Casting
 0.50 - 1.2 %0.50 - 1.2 %Addition, Ingot form
Iron, Fe <= 0.065 %<= 0.065 %Impurity, Ingot form
 <= 0.075 %<= 0.075 %Impurity, Casting
Lead, Pb <= 0.0050 %<= 0.0050 %Impurity, Ingot form
 <= 0.0060 %<= 0.0060 %Impurity, Casting
Magnesium, Mg 0.015 - 0.030 %0.015 - 0.030 %Addition, Casting
 0.020 - 0.030 %0.020 - 0.030 %Addition, Ingot form
Tin, Sn <= 0.0020 %<= 0.0020 %Impurity, Ingot form
 <= 0.0030 %<= 0.0030 %Impurity, Casting
Zinc, Zn 87.193 - 88.68 %87.193 - 88.68 %As balance; Ingot per ASTM B 669
 87.18 - 88.985 %87.18 - 88.985 %As balance; Castings per ASTM B 791
 
Descriptive Properties
Damping5.1 Q-1 x 103at 100 Hz, 20°C
 9.8 Q-1 x 103at 100 Hz, 100°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Die Cast
Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Die Cast
Aluminum 6061-T6; 6061-T651
Zinc ILZRO 16 (Zn-1.25Cu-0.2Ti-0.15Cr), Die Cast
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast

MZN12C / 14518

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.