Parts made from the mass-dyed polyamide 11 powder have a uniform black color and are therefore particularly suitable for visible areas that are subject to abrasive wear. In addition, they have high impact resistance and elongation at break and do not splinter even under the highest levels of mechanical stress. Compared to PA 12, they have higher temperature resistance and nearly constant mechanical properties over a wide temperature range. The material PA 1102 black is based on renewable resources (castor oil).Information provided by EOS GmbH (Electro Optical Systems). |