MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Avient Edgetek® NN-10GF-10CF-20MN/000 Nylon 66 - 10% Glass Fiber/10% Carbon Fiber/20% Mineral - ESD Applications  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Carbon Fiber Filled

Material Notes: Data provided by PolyOne.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Water Absorption 0.60 %0.60 %24 hrs. ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Thickness 3.17 mm
0.0030 - 0.0050 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 179 MPa26000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 11.7 GPa1700 ksiASTM D638
Izod Impact, Notched 0.690 J/cm
@Thickness 6.35 mm
1.29 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 ohm - 1e+051000 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 282 - 299 °C540 - 570 °FStock
Mold Temperature 66.0 - 107 °C151 - 225 °F
Drying Temperature 82.0 °C180 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Albis Plastics Polyamide 66 PA 910/1/ CF 10 GF10 HZ , 10% Carbon Fiber, 10% Glass Fiber, Impact Modified, DAM
RTP Company ESD A 201 Nylon 6/6 (PA), Glass Fiber - ESD Protection - Static Dissipative
RTP Company ESD A 204  Nylon 6/6 (PA 6/6) Dissipative - Glass Fiber 25%
RTP Company RTP 299 X 143540 D Nylon 6/6 (PA); ESD Protection - Permanently Anti-static - Glass Fiber - Preliminary Datasheet
Avient Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled

PHEH56 / 46448

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.