MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Mineral Filled

Material Notes: AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offers excellent dimensional stability and chemical resistance, good mechanical properties and low warpage, and moisture absorption.

This material is readily injection molded using conventional equipment and methods.

Information provided by Solvay Advanced Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
 1.49 g/cc1.49 g/ccISO 1183A
Moisture Absorption at Equilibrium 0.20 %0.20 %24 hours; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 125125ASTM D785
Tensile Strength, Yield 81.0 MPa11700 psiISO 527
 85.0 MPa12300 psiASTM D638
 20.0 MPa
@Temperature 175 °C
2900 psi
@Temperature 347 °F
ISO 527
 24.0 MPa
@Temperature 150 °C
3480 psi
@Temperature 302 °F
ISO 527
 41.0 MPa
@Temperature 100 °C
5950 psi
@Temperature 212 °F
ISO 527
Elongation at Break 1.9 %1.9 %ISO 527
 8.9 %
@Temperature 100 °C
8.9 %
@Temperature 212 °F
ISO 527
 12.3 %
@Temperature 175 °C
12.3 %
@Temperature 347 °F
ISO 527
 15 %
@Temperature 150 °C
15 %
@Temperature 302 °F
ISO 527
Elongation at Yield 2.1 %2.1 %ASTM D638
Tensile Modulus 5.80 GPa841 ksiISO 527
 6.10 GPa885 ksiASTM D638
 0.600 GPa
@Temperature 175 °C
87.0 ksi
@Temperature 347 °F
ISO 527
 0.700 GPa
@Temperature 150 °C
102 ksi
@Temperature 302 °F
ISO 527
 3.20 GPa
@Temperature 100 °C
464 ksi
@Temperature 212 °F
ISO 527
Flexural Strength 110 MPa16000 psiISO 178
 148 MPa21500 psiASTM D790
 15.0 MPa
@Temperature 175 °C
2180 psi
@Temperature 347 °F
ISO 178
 18.0 MPa
@Temperature 150 °C
2610 psi
@Temperature 302 °F
ISO 178
 60.0 MPa
@Temperature 100 °C
8700 psi
@Temperature 212 °F
ISO 178
Flexural Modulus 4.30 GPa624 ksiISO 178
 5.60 GPa812 ksiASTM D790
 0.600 GPa
@Temperature 175 °C
87.0 ksi
@Temperature 347 °F
ISO 178
 0.700 GPa
@Temperature 150 °C
102 ksi
@Temperature 302 °F
ISO 178
 3.30 GPa
@Temperature 100 °C
479 ksi
@Temperature 212 °F
ISO 178
Compressive Strength 162 MPa23500 psiASTM D695
Poissons Ratio 0.320.32
Shear Modulus 2.20 - 2.31 GPa319 - 335 ksiCalculated
Shear Strength 74.0 MPa10700 psiASTM D732
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inASTM D256
Izod Impact, Unnotched 6.94 J/cm13.0 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.90 kJ/m²2.81 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 53.0 kJ/m²25.2 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 4.90 J/cm²23.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.460 J/cm²2.19 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 313 °C595 °FASTM D3418
 313 °C595 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 154 °C309 °FASTM D648
 154 °C309 °FISO 75Af

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVT86 / 21382

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.