MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Propionate, Molded

Material Notes: Applications:
  • Appliances
  • Personal Care and Cosmetics

Product Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Propionate 360-16 has a plasticizer level of 16%.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 1.4 %
@Time 86400 sec
1.4 %
@Time 24.0 hour
Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6868ASTM D785
Tensile Strength at Break 30.3 MPa4390 psiASTM D638
Tensile Strength, Yield 26.9 MPa3900 psiASTM D638
Elongation at Break 45 %45 %ASTM D638
Flexural Strength 35.2 MPa5110 psiASTM D790
Flexural Modulus 1.241 GPa180.0 ksiASTM D790
Izod Impact, Notched  1.23 J/cm
@Temperature -40.0 °C
2.30 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 >= 5.33 J/cm
@Temperature 23.0 °C
>= 9.99 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 - 1.00e+15 ohm-cm1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.3 - 3.8
@Frequency 1e+6 Hz
3.3 - 3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 - 18.7 kV/mm300 - 475 kV/inASTM D149
Dissipation Factor 0.010 - 0.15
@Frequency 1e+6 Hz
0.010 - 0.15
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 - 170 µm/m-°C61.1 - 94.4 µin/in-°FASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°C0.301 - 0.399 BTU/lb-°FDSC
Thermal Conductivity 0.170 - 0.330 W/m-K1.18 - 2.29 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FASTM D648
Vicat Softening Point 92.0 °C198 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46 - 1.49
@Wavelength 589.3 nm
1.46 - 1.49
@Wavelength 589.3 nm
nD; ASTM D542
Haze <= 8.5 %<= 8.5 %ASTM D1003
Transmission, Visible >= 90 %>= 90 %ASTM E308
 
Descriptive Properties
Formula Number360
Plasticizer16 percent
Soluble Matter Loss0.1 percentASTM D570
Weight Loss on Heating1.3 percentASTM D707, 72 hrs, 80°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp

PE8835 / 129680

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.