MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2199 X 134911 A Polyetherimide (PEI) Nickel-Coated Carbon Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), Nickel Coated Graphite Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/ccASTM D 792
Linear Mold Shrinkage 0.00050 cm/cm
@Thickness 3.20 mm
0.00050 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 153 MPa22200 psiASTM D 638
Elongation at Break 1.2 %1.2 %ASTM D 638
Tensile Modulus 15.2 GPa2200 ksiASTM D 638
Flexural Strength 252 MPa36600 psiASTM D 790
Flexural Modulus 15.9 GPa2300 ksiASTM D 790
Izod Impact, Notched 0.961 J/cm
@Thickness 3.20 mm
1.80 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 4.00 J/cm
@Thickness 3.20 mm
7.50 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  65 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
65 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 68 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
68 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 73 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
73 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 77 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
77 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 80 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
80 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 82 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
82 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 82 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
82 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 88 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
88 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 89 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
89 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 94 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
94 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 96 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
96 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 97 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
97 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 206 °C403 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 371 - 399 °C700 - 750 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 14400 sec
300 °F
@Time 4.00 hour
Moisture Content 0.040 %0.040 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 2185  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 30%
RTP Company EMI 2184  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 25%
RTP Company EMI 2183  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 20%
RTP Company EMI 2162 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1382  Polyphenylene Sulfide (PPS) Shielding - Nickel-Coated Carbon Fiber 15%

PQZTA26591 / 159230

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.