MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

M-252 J1500 Nickel Superalloy
Categories: Metal; Superalloy; Nickel Base

Material Notes: Typical Applications: Gas turbine blades, parts, sheets

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.26 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  159 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
23000 psi
@Temperature 1500 °F,
Time 1000 hour
 255 MPa
@Temperature 816 °C,
Time 360000 sec
37000 psi
@Temperature 1500 °F,
Time 100 hour
 607 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
88000 psi
@Temperature 1200 °F,
Time 1000 hour
 703 MPa
@Temperature 649 °C,
Time 360000 sec
102000 psi
@Temperature 1200 °F,
Time 100 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.6 µm/m-°C
@Temperature 20.0 - 100 °C
5.89 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 11.7 W/m-K
@Temperature 20.0 - 100 °C
81.2 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.0 %1.0 %
Boron, B 0.0050 %0.0050 %
Carbon, C 0.15 %0.15 %
Chromium, Cr 19 %19 %
Cobalt, Co 10 %10 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni 66.245 %66.245 %As Balance
Silicon, Si <= 0.50 %<= 0.50 %
Titanium, Ti 2.6 %2.6 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alloy 713C Cast Nickel Superalloy (UNS N07713)
RTP Company RTP 1500-55D TFE 15 Polyether-Ester Block Copolymer (TEEE / COPE), PTFE Lubricated
301 Stainless Steel
DS-Niclel Nickel Superalloy Sheet
Chosun Refractories 1500 ACE BLANKET Blanket

NZ97021 / 191421

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.