Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Filler/Reinforcement: Mineral, 30% Filler by Weight Additive: Flame Retardant Features: Flame Retardant; Flame Retardant; UV Resistant Uses: Connectors; Electrical/Electronic Applications RoSH Compliance: RoSH Compliant Forms: Granules Processing Method: Injection Molding Information provided by EMS-Grivory |