MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Morgan Advanced Ceramics Teraglide™ Titania
Categories: Ceramic; Oxide; Titanium Oxide

Material Notes: Special material that is electrically-insulative in pure form or electrically-conductive in reduced form. Used for threadguides in high-speed processing of synthetic fibres.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.10 g/cc0.148 lb/in³Fired
Porosity 0.00 %0.00 %Apparent, fully dense
Particle Size <= 2.0 µm<= 2.0 µmGrain size
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 98009800MPa, at Hv 0.5kg
Flexural Strength 350 MPa50800 psi3-point
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm
@Temperature 20.0 °C
>= 1.00e+12 ohm-cm
@Temperature 68.0 °F
pure
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.80 µm/m-°C
@Temperature 20.0 °C
4.89 µin/in-°F
@Temperature 68.0 °F
 8.80 µm/m-°C
@Temperature 800 °C
4.89 µin/in-°F
@Temperature 1470 °F
Thermal Conductivity 5.00 W/m-K
@Temperature 20.0 °C
34.7 BTU-in/hr-ft²-°F
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORG33 / 90411

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.