System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Mineral Filled
Material Notes:
Plate-able. Natural and colors available. Injection molding grade.
Uses: Automotive, appliances
Information provided by Engineered Polymer Solutions.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.50
g/cc
0.0542
lb/in³
ASTM D792-91
Viscosity Measurement
1500
@Temperature 250 °C
1500
@Temperature 482 °F
in-sec Melt Viscosity; 5.0 kg; ASTM D1238 Mod.
Linear Mold Shrinkage
0.012
cm/cm
0.012
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
57.9
MPa
8400
psi
ASTM D638
Flexural Modulus
4.14
GPa
600
ksi
ASTM D790
Izod Impact, Notched
0.427
J/cm
0.800
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
188
°C
370
°F
1/4 inch bar; ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
238
-
254
°C
460
-
490
°F
Middle Barrel Temperature
243
-
260
°C
470
-
500
°F
Front Barrel Temperature
249
-
266
°C
480
-
510
°F
Nozzle Temperature
243
-
260
°C
470
-
500
°F
Melt Temperature
249
-
266
°C
480
-
510
°F
Mold Temperature
71.1
-
93.3
°C
160
-
200
°F
Drying Temperature
121
°C
250
°F
Dry Time
3
-
4
hour
3
-
4
hour
Moisture Content
0.20 %
0.20 %
Back Pressure
0.345
-
0.689
MPa
50.0
-
100
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Gromax PBT 4130-104D 30% Glass Fiber Filled
PEPS10 / 36413
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.