MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Compounding Resin

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for efficient blending with pigments, slip additives and antiblock additives.

Applications: Color concentrates; Slip and antiblock masterbatches.

Key Words: Linear Low Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³Exxon Method
Environmental Stress Crack Resistance 250 hour250 hourF50, Igepal, Condition C; ASTM D-1693
Melt Flow 22 g/10 min22 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ASTM D2240
Tensile Strength, Ultimate 20.0 MPa2900 psiASTM D638
Tensile Strength, Yield 12.0 MPa1740 psiASTM D638
Elongation at Break 345 %345 %
Flexural Modulus 0.335 GPa48.6 ksiASTM D790
Tensile Impact Strength 84.0 kJ/m²40.0 ft-lb/in²23°C; ASTM D-1822
Dart Drop, Total Energy 29.0 J
@Temperature -40.0 °C
21.4 ft-lb
@Temperature -40.0 °F
F50; ASTM D-3029
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °FExxon Method
Brittleness Temperature -68.0 °C-90.4 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXCGI / 37966

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.