MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Chemical Concepts ChemSet™ 355 Silicone Potting Material, Black
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: ChemSet 355 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readily repairable. Key Features: 100% solids – no solvents. Long pot life, Low modulus, Good elongation, UL 94 V-0 rated, file number: QMFZ2.E205830.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/cc335A, uncatalyzed
 1.63 g/cc1.63 g/cc335B, uncatalyzed
Viscosity 6000 cP6000 cP335A, uncatalyzed
 6000 cP6000 cP335B, uncatalyzed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545Cured, 15 minutes @ 150°C
Tensile Strength 1.72 MPa250 psiCured, 15 minutes @ 150°C
100% Modulus 1.24 MPa
@Strain 100 %,
Temperature 150 °C
180 psi
@Strain 100 %,
Temperature 302 °F
cured, 15 minutes
Tear Strength Test 45
@Temperature 150 °C
45
@Temperature 302 °F
cured, 15 minutes
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.02e+14 ohm-cm4.02e+14 ohm-cm
Dielectric Constant 3.08
@Frequency 1000 Hz
3.08
@Frequency 1000 Hz
Dissipation Factor 0.00900.0090
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.680 W/m-K4.72 BTU-in/hr-ft²-°Fhot wire method
Maximum Service Temperature, Air 240 °C464 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Working Life 100 min
@Temperature 25.0 °C
100 min
@Temperature 77.0 °F
 
Descriptive Properties
Color335A, beige, uncatalyzed
 335B, black, uncatalyzed
Mix Ratio1:1
Performance Level Category (PLC)0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-BOND® 1038 Conductive Silicone RTV Adhesive
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Fast Cure Silicone Rubber
Dow Q2-7406 ADHESIVE
Dow JCR 6110 A/B
Dow HIPEC® Q3-6645 SEMICONDUCTOR PROTECTIVE COATING KIT

PCHEMI902 / 232176

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.