MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Titanium, high purity
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes:

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.51 g/cc0.163 lb/in³alpha
 4.35 g/cc
@Temperature 885 °C
0.157 lb/in³
@Temperature 1630 °F
beta
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 9090increases with impurities
Hardness, Knoop 9999Estimated from Brinell.
Hardness, Vickers 100100increases with impurities
Modulus of Elasticity 105 GPa15200 ksi
Poissons Ratio 0.32 - 0.360.32 - 0.36
Fatigue Strength 130 MPa
@# of Cycles 1.00e+6
18900 psi
@# of Cycles 1.00e+6
Shear Modulus 39.2 GPa5690 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000450 ohm-cm0.0000450 ohm-cm
Magnetic Susceptibility 0.000003170.00000317cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 325 J/g140 BTU/lb
CTE, linear 8.41 µm/m-°C
@Temperature 20.0 °C
4.67 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.523 J/g-°C0.125 BTU/lb-°F
Thermal Conductivity 17.0 W/m-K118 BTU-in/hr-ft²-°F
Melting Point 1670 °C3040 °F
Liquidus 1660 °C3020 °F
Beta Transus 882 °C1620 °FHeat of transition is 85 J/g
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.30
@Temperature 710 °C
0.30
@Temperature 1310 °F
Reflection Coefficient, Visible (0-1) 0.560.56Visible
 
Component Elements PropertiesMetricEnglishComments
Titanium, Ti 100 %100 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 1
Titanium Grade 2
Titanium Grade 7
Titanium Grade 3
Titanium Grade 11

MTUHP0 / 14270

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.