MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Braskem AC59 HDPE Monofilament Polyethylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); HDPE, Fiber Grade

Material Notes: AC59 resin is a high-density polyethylene homopolymer produced by the solution process and designed for monofilament applications. It contains antioxidant additives. Its applications include: film extrusion, monofilament, raffia, raschel, nets, oriented structures, and general use. Processing Conditions for Oriented Structures: cast film - typical temperature profile: 170 to 220ºC; blown film - typical temperature profile: 170 to 220ºC; monofilament - typical temperature profile: 170 to 220ºC. Typical Stretch Ratio: 4 to 8:1.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM-D792
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959ASTM-D2240
Tensile Strength at Break 35.0 MPa5080 psiASTM-D638
Tensile Strength, Yield 28.0 MPa4060 psiASTM-D638
Elongation at Break 2036 %2036 %ASTM-D638
Elongation at Yield 11 %11 %ASTM-D638
Flexural Modulus, 1% Secant 1180 MPa171000 psiASTM-D790
Izod Impact, Notched 1.75 J/cm3.28 ft-lb/inASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C162 °FASTM-D648
Vicat Softening Point 127 °C
@Load 1.02 kg
261 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem BU 004 HDPE Blow Molding Polyethylene
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer
Braskem GP5550 HDPE High Density Extrusion Polyethylene
Braskem GM7746CA HDPE Blow Molding Polyethylene
Braskem AD57 HDPE Monofilament Polyethylene Copolymer

PBRAS872 / 106718

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.