MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP PA66 TRM black 1015061 Nylon 66, Carbon Fiber Reinforced, PTFE Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Carbon Fiber/PTFE Filled

Material Notes:
  • very good bearing and wear properties
Target Industries:
  • automotive industry
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 g/cc0.0231 lb/in³EN ISO 60
Density 1.30 g/cc0.0470 lb/in³
Water Absorption at Saturation 1.9 %1.9 %50 % relative humidity up to saturation; DIN EN ISO 62
Viscosity Number 150 cm³/g1.5 dl/gsolution 0,005 g/ml sulphuric acid; DIN EN ISO 307
Linear Mold Shrinkage, Flow 0.0037 cm/cm0.0037 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0104 cm/cm0.0104 in/inDIN EN ISO 294-4
Melt Flow 57 g/10 min
@Load 5.00 kg,
Temperature 280 °C
57 g/10 min
@Load 11.0 lb,
Temperature 536 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 150 MPa21800 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 3.0 %3.0 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 9.00 GPa1310 ksi50 mm/min; DIN EN ISO 527-1
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²DIN EN ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1300 ohm-cm1300 ohm-cmDIN EN ISO 3915
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  22.0 µm/m-°C
@Temperature 70.0 - 120 °C
12.2 µin/in-°F
@Temperature 158 - 248 °F
DIN EN ISO 11359-1;2
 24.0 µm/m-°C
@Temperature 23.0 - 45.0 °C
13.3 µin/in-°F
@Temperature 73.4 - 113 °F
DIN EN ISO 11359-1;2
CTE, linear, Transverse to Flow  108 µm/m-°C
@Temperature 23.0 - 45.0 °C
60.0 µin/in-°F
@Temperature 73.4 - 113 °F
DIN EN ISO 11359-1;2
 142 µm/m-°C
@Temperature 70.0 - 120 °C
78.9 µin/in-°F
@Temperature 158 - 248 °F
DIN EN ISO 11359-1;2
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°Fthrough-plane; ISO 22007-4:2008
 0.600 W/m-K4.16 BTU-in/hr-ft²-°Fin-plane; ISO 22007-4:2008
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 110 °C230 °Flong term
 170 °C338 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO-R 75 Method A
Glass Transition Temp, Tg 5.00 °C41.0 °Fmoist; DIN 53765
 72.0 °C162 °Fdry; DIN 53765
Flammability, UL94 HBHBDIN IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 - 300 °C536 - 572 °FCylinder
Melt Temperature 290 - 300 °C554 - 572 °FMaterial temperature
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9036 / 318964

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.