MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mocom (ALBIS) ALCOM® PPA 930/1 GF30 PTFE15 PPA, 30/15% Glass/PTFE Reinforced
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Glass/PTFE Filled

Material Notes: Base Polymer: Polyphthalamide

Filler/Additive System: 30% glass fibers, 15% PTFE

Special Features: Improved sliding/wear

Market Segment: Automotive, Machinery

Application Area: Functional components

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Time 86400 sec
0.0020 - 0.0040 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Time 86400 sec
0.0050 - 0.0070 in/in
@Time 24.0 hour
ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 164 MPa23800 psiISO 527
Elongation at Break 1.9 %1.9 %ISO 527
Tensile Modulus 11.0 GPa1600 ksiISO 527
Flexural Strength 235 MPa34100 psiISO 178
Flexural Modulus 9.50 GPa1380 ksiISO 178
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 285 °C545 °FISO 75-1/-2
Vicat Softening Point 264 °C507 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 345 °C608 - 653 °FInjection molding
Mold Temperature 135 - 145 °C275 - 293 °FInjection molding
Drying Temperature 110 - 130 °C
@Time 14400 - 28800 sec
230 - 266 °F
@Time 4.00 - 8.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyphthalamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
E-Polymers SEPAZ® V215A 15% Glass Fiber Reinforced PPA
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Conditioned, 30% Glass Filled

PALBIS8197 / 242256

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.