MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mitsui AURUM® PL450C Polyimide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Material Notes: AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURUM PL450C offers a unique balance of mechanical and thermal properties for superior performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM exhibits outstanding resistance to chemicals and radiation, a low coefficient of thermal expansion, ultrahigh purity, low outgassing in a vacuum, excellent electrical properties, and flame resistance. AURUM PL450C can be conventionally extruded to produce high performance wire & cable insulation, thin-wall tubing, and fiber.

Applications: AURUM PL450C injection molded components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM PL450C parts include heat-resistant gears, seals, ferrules and other fasteners, coil bobbins, semiconductor manufacturing and handling equipment components, and thermal and electrical insulators. Products produced from extruded AURUM PL450C resin include thin-wall tubing, wire and cable insulation, monofilament, and rod stock shapes.

Information provided by DuPont

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Water Absorption 0.34 %0.34 %24 hrs @ 73°F; ASTM D570
Moisture Absorption at Equilibrium 0.24 %0.24 %73°F; 60 RH, 24hrs
Linear Mold Shrinkage 0.0083 cm/cm0.0083 in/inASTM D955
Melt Flow 4.5 - 7.5 g/10 min
@Load 1.05 kg,
Temperature 400 °C
4.5 - 7.5 g/10 min
@Load 2.31 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 92.18 MPa13370 psiASTM D638
 57.9 MPa
@Temperature 149 °C
8400 psi
@Temperature 300 °F
ASTM D638
Elongation at Yield 90 %90 %ASTM D638
 90 %
@Temperature 149 °C
90 %
@Temperature 300 °F
ASTM D638
Modulus of Elasticity 2.76 GPa400 ksiASTM D882
Flexural Strength 137 MPa19900 psiASTM D790
 88.3 MPa
@Temperature 149 °C
12800 psi
@Temperature 300 °F
ASTM D790
Flexural Modulus 2.943 GPa426.8 ksiASTM D790
 2.550 GPa
@Temperature 149 °C
369.9 ksi
@Temperature 300 °F
ASTM D790
Compressive Strength  76.5 MPa
@Temperature 149 °C
11100 psi
@Temperature 300 °F
JIS K7208
 119.7 MPa
@Temperature 22.8 °C
17360 psi
@Temperature 73.0 °F
JIS K7208
Izod Impact, Notched 0.908 J/cm1.70 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cm1.00e+17 - 1.00e+18 ohm-cmASTM D257
Surface Resistance 1.00e+17 - 1.00e+18 ohm1.00e+17 - 1.00e+18 ohmASTM D257
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
ASTM D150
 3.2
@Frequency 1000 Hz
3.2
@Frequency 1000 Hz
ASTM D150
Dissipation Factor  0.00090
@Frequency 1000 Hz
0.00090
@Frequency 1000 Hz
ASTM D150
 0.0034
@Frequency 1e+6 Hz
0.0034
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  54.0 µm/m-°C
@Temperature 22.8 °C
30.0 µin/in-°F
@Temperature 73.0 °F
MD; ASTM D696
 54.0 µm/m-°C
@Temperature 73.0 °C
30.0 µin/in-°F
@Temperature 163 °F
TD; ASTM D696
Specific Heat Capacity 1.00 J/g-°C0.240 BTU/lb-°FDSC
 1.004 J/g-°C
@Temperature 100 °C
0.2400 BTU/lb-°F
@Temperature 212 °F
DSC
 1.423 J/g-°C
@Temperature 300 °C
0.3400 BTU/lb-°F
@Temperature 572 °F
DSC
Thermal Conductivity 0.174333 W/m-K1.20987 BTU-in/hr-ft²-°FASTM C177
Melting Point 388 °C730 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 238 °C460 °FASTM D648
Glass Transition Temp, Tg 250 °C482 °FDSC
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 5VA
@Thickness 2.00 mm
5VA
@Thickness 0.0787 in
Oxygen Index 47 %
@Thickness 3.20 mm
47 %
@Thickness 0.126 in
ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline
Solvay CYCOM® 2237 Polyimide Resin System
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled

PMIT045E / 53226

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.