MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Delrin® 500CPE NC010 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Medium Viscosity Acetal Homopolymer with Improved Processing and Very Low Emissions

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Melt Density 1.19 g/cc
@Temperature 205 °C
0.0430 lb/in³
@Temperature 401 °F
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4, 2577
Melt Flow  13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric; ISO 1133
 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 72.0 MPa10400 psiISO 527-1/-2
Elongation at Break 33 %33 %Nominal; ISO 527-1/-2
Elongation at Yield 16 %16 %ISO 527-1/-2
Tensile Modulus 3.10 GPa450 ksiISO 527-1/-2
Flexural Strength 93.0 MPa13500 psiISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Poissons Ratio 0.370.37
Charpy Impact Unnotched  >= 25.0 J/cm²
@Temperature 23.0 °C
>= 119 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 34.0 J/cm²
@Temperature -30.0 °C
162 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 20.0 mm/min
@Thickness 1.00 mm
0.787 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 °C401 °FOptimum, Injection
 200 - 210 °C392 - 410 °FRange, Injection
Mold Temperature 90.0 °C194 °FOptimum, Injection
 80.0 - 100 °C176 - 212 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 80.0 - 100 MPa11600 - 14500 psiInjection
 100 MPa14500 psiInjection
Annealing Temperature 160 °C320 °FOptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Emissions (mg/kg)<2VDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.3Injection
Part Marking Code>POM<ISO 11469
PolymerPOM
Processing Hold Pressure Time (s/mm)8Injection
Resin IdentificationPOMISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5117c / 254327

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.