MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ATI Wah Chang Nb/Nb Alloy Nb-I ZR
Categories: Metal; Nonferrous Metal; Niobium Alloy

Material Notes: Improved creep strength versus pure niobium. Replacement for pure niobium in applications requiring the chemical resistance of niobium and a material with high melting temperature.

Information provided by ATI Wah Chang

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.58 g/cc0.310 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 68.98 GPa
@Temperature 23.0 °C
10000 ksi
@Temperature 73.4 °F
Charpy Impact 210 J
@Temperature 23.0 °C
155 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 41.85 W/m-K290.4 BTU-in/hr-ft²-°F
Melting Point 2400 - 2420 °C4350 - 4390 °F
Solidus 2400 °C4350 °F
Liquidus 2420 °C4390 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1)  0.103
@Temperature 500 °C
0.103
@Temperature 932 °F
Total Hemispherical
 0.11
@Temperature 600 °C
0.11
@Temperature 1110 °F
Total Hemispherical
 0.117
@Temperature 700 °C
0.117
@Temperature 1290 °F
Total Hemispherical
 0.13
@Temperature 800 °C
0.13
@Temperature 1470 °F
Total Hemispherical
 0.142
@Temperature 900 °C
0.142
@Temperature 1650 °F
Total Hemispherical
 0.154
@Temperature 100 °C
0.154
@Temperature 212 °F
Total Hemispherical
 0.167
@Temperature 1100 °C
0.167
@Temperature 2010 °F
Total Hemispherical
 0.179
@Temperature 1200 °C
0.179
@Temperature 2190 °F
Total Hemispherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Niobium 56/Titanium 44 Alloy
ATI Wah Chang Nb/Nb Alloy C-103
Elmet-Starck 2602 Molybdenum Powder Metallurgy Alloy ODS Mo-La
Niobium, Nb; High Purity
Niobium, Nb; Soft

NATIWC03 / 15058

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.