Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Material Notes:
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.52
g/cc
1.52
g/cc
ASTM D792
Density
1.51
g/cc
0.0546
lb/in³
ISO 1183
Water Absorption
<= 0.10 %
@Temperature 22.8 °C
<= 0.10 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow
0.0030
-
0.0040
cm/cm
0.0030
-
0.0040
in/in
ASTM D955
0.0030
-
0.0060
cm/cm
0.0030
-
0.0060
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0098
cm/cm
0.0098
in/in
ISO 294-4
Melt Flow
12
-
30
g/10 min
12
-
30
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
85.0
MPa
12300
psi
5mm/min; ISO 527-2/1A
86.2
MPa
12500
psi
ASTM D638
Elongation at Break
2.1 %
2.1 %
5mm/min; ISO 527-2/1A
3.0 %
3.0 %
ASTM D638
Tensile Modulus
8.00
GPa
1160
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
138
MPa
20000
psi
ASTM D790
140
MPa
20300
psi
ISO 178
Flexural Modulus
6.89
GPa
1000
ksi
ASTM D790
8.00
GPa
1160
ksi
ISO 178
Izod Impact, Notched
0.587
J/cm
1.10
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
6.20
kJ/m²
2.95
ft-lb/in²
ISO 180/1A
Charpy Impact, Notched
0.600
J/cm²
2.86
ft-lb/in²
ISO 179/1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
19.0
µm/m-°C
10.6
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
70.0
µm/m-°C
38.9
µin/in-°F
ISO 11359-2
Melting Point
225
°C
437
°F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
209
°C
408
°F
ISO 75-1, -2
212
°C
414
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
172
°C
342
°F
ISO 75-1, -2
175
°C
347
°F
ASTM D648
Flammability, UL94
HB
HB
Processing Properties
Metric
English
Comments
Processing Temperature
65.0
-
96.0
°C
149
-
205
°F
cavity
250
-
265
°C
482
-
509
°F
hot runner
Feed Temperature
230
-
250
°C
446
-
482
°F
Zone 1
230
-
250
°C
446
-
482
°F
Zone 2
235
-
255
°C
455
-
491
°F
Zone 3
235
-
255
°C
455
-
491
°F
Zone 4
240
-
265
°C
464
-
509
°F
Die Temperature
240
-
265
°C
464
-
509
°F
Melt Temperature
235
-
265
°C
455
-
509
°F
260
°C
500
°F
ISO 294
Mold Temperature
82.0
°C
180
°F
ISO 294
Injection Velocity
300
mm/sec
11.8
in/sec
ISO 294
Drying Temperature
120
-
130
°C
248
-
266
°F
Dry Time
4.00
hour
4.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Hold Pressure
48.0
MPa
6960
psi
ISO 294
Descriptive Properties
Injection molding
Yes
Injection speed
medium-fast
Processing conditions acc. ISO
7792-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PHCQ083 / 178538
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.