MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet
Categories: Polymer; Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 - 1.80 g/cc1.60 - 1.80 g/ccIEC 1212-2 8.1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 100 MPa>= 14500 psiIEC 1212-2 5.7
Flexural Strength >= 140 MPa>= 20300 psiPerpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 14.0 GPa>= 2030 ksiIEC 1212-2 5.2
Izod Impact, Unnotched (ISO) >= 29.0 kJ/m²>= 13.8 ft-lb/in²Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 2.50 J/cm²>= 11.9 ft-lb/in²Parallel to laminations; IEC 1212-2 5.5.2
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+8 ohm>= 1.00e+8 ohmAfter immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.0
@Frequency 48.0 - 62.0 Hz
<= 5.0
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 20000 V
@Temperature 90.0 °C
>= 20000 V
@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Comparative Tracking Index >= 100 V>= 100 VIEC 1212-2 6.4
 
Descriptive Properties
Thermal Endurance120 T.I.IEC 1212-2 7.1
Water Absorption< 310 mgIEC 1212-2 8.2; Test piece 50 x 50 x 10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hanwha Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix

PHIPPE924 / 121928

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.