MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Celanex® 7700 Polyester (PBT), 35% Glass/Mineral
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Flame retardant and low warp

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.74 g/cc0.0629 lb/in³ASTM D792
Water Absorption 0.040 %0.040 %ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7676ISO 2039-2
Tensile Strength, Ultimate 90.0 MPa13100 psiISO 527
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 150 MPa21800 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Izod Impact, Notched (ISO) 4.30 kJ/m²2.05 ft-lb/in²ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
Dielectric Strength 24.0 kV/mm
@Thickness 3.17 mm
610 kV/in
@Thickness 0.125 in
50% R.H.; ASTM D149
Dissipation Factor 0.0090
@Frequency 100 Hz
0.0090
@Frequency 100 Hz
Comparative Tracking Index 300 V300 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 223 °C433 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 204 °C399 °FISO 75
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
UL94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Vandar® 8929 Thermoplastic Polyester Alloy
Celanese Vandar® 2100 PBT, Unfilled

PHCT35 / 45675

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.