MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

United Cast Bar Unibar 350 Continuously Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a good surface finish. Noise and vibration damping are good in this grade.

Unibar-350 can be hardened by conventional methods, to Rc 50 on the bar surface.

Information provided by United Cast Bar Ltd.

Key Words: EN-1561-GJL-350 GG35; Meehanite GA350
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.30 g/cc0.264 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 230 - 300
@Load 3000 kg
230 - 300
@Load 6610 lb
10 mm ball
Tensile Strength  225 MPa
@Diameter 150 - 300 mm
32600 psi
@Diameter 5.91 - 11.8 in
 250 MPa
@Diameter 80.0 - 150 mm
36300 psi
@Diameter 3.15 - 5.91 in
 280 MPa
@Diameter 40.0 - 80.0 mm
40600 psi
@Diameter 1.57 - 3.15 in
 315 MPa
@Diameter 20.0 - 40.0 mm
45700 psi
@Diameter 0.787 - 1.57 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.95 - 3.45 %2.95 - 3.45 %
Iron, Fe 92.58 - 94.21 %92.58 - 94.21 %as balance
Manganese, Mn 0.60 - 0.80 %0.60 - 0.80 %
Phosphorus, P 0.10 - 0.20 %0.10 - 0.20 %
Silicon, Si 2.1 - 2.9 %2.1 - 2.9 %
Sulfur, S 0.040 - 0.070 %0.040 - 0.070 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
United Cast Bar Unibar 200 Continuously Cast Iron
Gray Cast Iron, ASTM A 48 Class 40
ASTM class 20 Standard gray iron test bars, as cast
United Cast Bar Unibar 250 Continuously Cast Iron
Overview of materials for Gray Cast Iron

NUNITED04 / 160451

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.