MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Tenite 572E3720012 Cellulose Acetate Butyrate, Clear, Trsp
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Butyrate, Molded

Material Notes: Applications:
  • Films
  • Profiles
  • Sheet

Product Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucents. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Butyrate 572-12 contains an odor mask lubricant and an ultra-violet inhibitor(UVI). It has a plasticizer level of 12%.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 1.3 %
@Time 86400 sec
1.3 %
@Time 24.0 hour
Immersion; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8787ASTM D785
Tensile Strength at Break 34.0 MPa4930 psiASTM D638
Tensile Strength, Yield 33.8 MPa4900 psiASTM D638
Elongation at Break 23 %23 %ASTM D638
Flexural Modulus 1.30 GPa189 ksiASTM D790
Izod Impact, Notched  0.980 J/cm
@Temperature -40.0 °C
1.84 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 3.48 J/cm
@Temperature 23.0 °C
6.52 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Descriptive Properties
Formula Number572UVI; odor mask
Plasticizer12 percent
Weight Loss on Heating0.4 percentASTM D707, 72 hrs, 80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate

PE8831 / 129676

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.