MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Rynite® 940 BK505 PET-(GF+MD)40
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Material Notes: 40% Glass/Mineral Reinforced Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 g/cc0.0592 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiISO 527-1/-2
Elongation at Break 1.8 %1.8 %ISO 527-1/-2
Tensile Modulus 12.5 GPa1810 ksiISO 527-1/-2
Flexural Modulus 13.0 GPa1890 ksiISO 178
Poissons Ratio 0.330.33
Charpy Impact Unnotched  3.50 J/cm²
@Temperature -40.0 °C
16.7 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -40.0 °C
2.86 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 62631-3-2
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 33.0 kV/mm838 kV/inIEC 60243-1
Dissipation Factor  0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
IEC 62631-2-1
 0.0146
@Frequency 1e+6 Hz
0.0146
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°FISO 11359-1/-2
 6.00 µm/m-°C
@Temperature 55.0 - 160 °C
3.33 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
 22.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
12.2 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
 54.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
30.0 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 84.0 µm/m-°C
@Temperature 55.0 - 160 °C
46.7 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
Melting Point 250 °C482 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 241 °C466 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 °C545 °FOptimum, Injection
 280 - 300 °C536 - 572 °FRange, Injection
Mold Temperature 110 °C230 °FOptimum, Injection
 100 - 120 °C212 - 248 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %<= 0.020 %Injection
Hold Pressure >= 80.0 MPa>= 11600 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-(GF+MD)40<ISO 11469
PolymerPET-(GF+P)40
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
 North America
 South and Central America
Resin IdentificationPET-(GF+MD)40ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GEHR Plastics Ultem® 2300 PEI-30 GF, 30% Glass Fiber Reinforced
Envalior Arnite® TV4 491 (PBT+PET)-GF50
Envalior Arnite® TV4 461 KL (PBT+PET)-GF30
Envalior Arnite® TV4 461 (PBT+PET)-GF30
Envalior Arnite® A02 307 PET

PDSX5267 / 197907

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.