MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)
Categories: Polymer; Film; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³
Thickness 60.0 microns2.36 mil
Melt Flow 3.0 g/10 min
@Load 2.16 kg
3.0 g/10 min
@Load 4.76 lb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 24.7 MPa3580 psiMolded property
Film Tensile Strength at Yield, MD 8.60 MPa1250 psi
Film Tensile Strength at Yield, TD 8.30 MPa1200 psi
Tensile Strength, Yield 9.50 MPa1380 psiMolded property
Film Elongation at Break, MD 515 %515 %
Film Elongation at Break, TD 545 %545 %
Elongation at Break 510 %510 %Molded value
Tensile Modulus 0.124 GPa18.0 ksi
Elmendorf Tear Strength MD 380 g380 g
Elmendorf Tear Strength TD 500 g500 g
Elmendorf Tear Strength, MD 6.30 g/micron160 g/mil
Elmendorf Tear Strength, TD 8.30 g/micron211 g/mil
Dart Drop 7.10 g/micron180 g/mil
Film Tensile Strength at Break, MD 37.9 MPa5500 psi
Film Tensile Strength at Break, TD 39.3 MPa5700 psi
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 78.0 °C172 °F
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %
Gloss 65 %65 %45°
 
Processing PropertiesMetricEnglishComments
Processing Temperature 191 °C376 °FFilm extrusion temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Dow Primacor® 2912 Ethylene Acrylic Acid (EAA)
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA)
Dow Primacor® 3150 Ethylene Acrylic Acid (EAA)
Dow Primacor® 3460 Ethylene Acrylic Acid (EAA)

PDW522 / 34591

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.