MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Insulcast® RTVS 3-95-1 Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST RTVS 3-95-1 is a low viscosity, thermally conductive RTV silicone compound, UL recognized under file E86165 for flame class 94V-0.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccUncured. Part B
 2.35 g/cc2.35 g/ccUncured. Part A
Viscosity 1000 cP1000 cPUncured. Part B; ASTM D2393
 10000 cP10000 cPMixed, Part A, Part B; ASTM D2393
 15000 cP15000 cPPart A; ASTM D2393
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ASTM D2240
Tensile Strength 3.28 MPa475 psiASTM D412
Elongation at Break 45 %45 %ASTM D412
Tear Strength 2.63 kN/m15.0 pliDie B; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+14 ohm-cm5.00e+14 ohm-cmASTM D257
Dielectric Constant 5.0
@Frequency 1000 Hz
5.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.0050
@Frequency 1000 Hz
0.0050
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 180 µm/m-°C100 µin/in-°F
Thermal Conductivity 1.25 W/m-K8.68 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 125 °C
0.250 hour
@Temperature 257 °F
option
 60.0 min
@Temperature 90.0 °C
1.00 hour
@Temperature 194 °F
option
 240 min
@Temperature 50.0 °C
4.00 hour
@Temperature 122 °F
option
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
option
Pot Life  90.0 min
@Temperature 25.0 °C
90.0 min
@Temperature 77.0 °F
Part A. 100 g
 90.0 min
@Temperature 25.0 °C
90.0 min
@Temperature 77.0 °F
Part B. 100g
Shelf Life 12.0 Month12.0 MonthPart A
 12.0 Month12.0 MonthPart B
 
Descriptive Properties
Colorclearpart B, uncured
 redpart A, uncured
Mix Ratio by weight100:5Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives CoolTherm™ SC-252 Silicone encapsulant system
Lord Adhesives CoolTherm™ SC-104 Thermally Conductive Silicone Encapsulant
Lord Adhesives Circalok™ 6703A/B Thermally Conductive Two Part Silicone, Flame Retardant
ITW Insulcast® RTVS 3-95-2 Silicone Potting/Encapsulation Compound
ITW Insulcast® RTVS 27 HTC Silicone Potting/Encapsulation Compound

PITWIN9113 / 239623

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.