MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Keysor-Century KYNS PVC Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: A solution grade, high molecular weight vinyl chloride-vinyl acetate copolymer resin. 10% Vinyl acetate. KYNS is soluble in strong ketone systems to produce low solution rheological properties, and is highly resistant to moisture, wear, and chemicals. White Free Flowing Powder

Recommended for printing ink, top coat applications to vinyl film and sheeting, architectural finishes for masonry, wood, and steel, and for coatings that require high resistance to moisture, wear, or chemicals.

Particle size: Nil retained on 32 mesh. 40% max through 200 mesh. Max volatiles 1%

Property values are typical values. Information provided by Keysor-Century Corporation.

Keysor-Century Corporation is no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Apparent Bulk Density 0.630 g/cc0.0228 lb/in³ASTM D1895
Brookfield Viscosity <= 300 cP
@Temperature 25.0 °C
<= 300 cP
@Temperature 77.0 °F
15% resin solution in MIBK: toluene [2:1 ratio], @ 30rpm
Viscosity Measurement 1.841.84Relative viscosity; ASTM D-1243

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Formosa Plastics Formolon® 113 PVC
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Inovyn 460SL Polyvinyl Chloride grafted copolymer

PKCV07 / 48700

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.