MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Clariant Renol PPOSP0001 Polyphenylene Oxide, Mineral Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Mineral Filled

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.62 g/cc1.62 g/ccASTM D792
Filler Content 50 %50 %ASTM D2584
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.3 MPa7300 psiASTM D638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D638
Flexural Yield Strength 110 MPa16000 psiASTM D790
Flexural Modulus 11.7 GPa1700 ksiASTM D790
Izod Impact, Notched 0.160 J/cm
@Temperature 22.8 °C
0.300 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C225 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 288 °C500 - 550 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Dry Time 3 - 4 hour
@Temperature 93.3 °C
3 - 4 hour
@Temperature 200 °F
Injection Pressure 41.4 - 74.5 MPa6000 - 10800 psiSecondary
 68.9 - 124 MPa10000 - 18000 psiInitial
Back Pressure 0.345 - 1.72 MPa50.0 - 250 psi
Shot Size 30 - 80 %30 - 80 %
Screw Speed 20 - 100 rpm20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Altron™ PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet)
GEHR Plastics Noryl PPO-30 GF 30% Glass Filled
GEHR Plastics Noryl PPO
E-Polymers TEKAPPO® J930 30% Glass Fiber Reinforced M-PPO
EPICHEM Epiryl PPO V0 Polyphenylene oxide

PCLAR174 / 82299

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.