MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Old Hickory No. 1 Glaze Kentucky Ball Clay
Categories: Ceramic; Clay; Ball Clay

Material Notes: No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high percentage of frit which has soluble alkali. No. Glaze provides viscosity control range and excellent rheology for all glaze application methods and especially bell or cone applications processes.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.37 µm0.37 µmMedian particle diameter
 0.50 µm0.50 µm52% of particles less than
 1.0 µm1.0 µm63% of particles less than
 <= 5.0 µm<= 5.0 µm87% of particles less than
pH 5.95.9
Soluble Sulfates 160 ppm160 ppm
Specific Surface Area 18 m²/g18 m²/g
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.90 µm/m-°C
@Temperature 50.0 - 500 °C
3.28 µin/in-°F
@Temperature 122 - 932 °F
Pre-fired 1200°C
Shrinkage 5.8 %5.8 %Linear Drying Shrinkage
 
Component Elements PropertiesMetricEnglishComments
Al2O3 29.37 %29.37 %
CaO 0.10 %0.10 %
Carbon, C 0.080 %0.080 %
Fe2O3 0.87 %0.87 %
K2O 0.28 %0.28 %
Kaolinite 70.8 %70.8 %
Loss on Ignition(%) 9.91 %9.91 %
MgO 0.28 %0.28 %
Na2O 0.10 %0.10 %
Quartz 22.4 %22.4 %
SiO2 56.32 %56.32 %
Sulfur, S 0.000073 %0.000073 %
TiO2 2.44 %2.44 %
 
Descriptive Properties
CEC/MBI (meg/100 ml)7.1
Crude ColorWhite
Dry Sieve Residue (%)0.4Dry Sieve Residue, +80 mesh
Feldspar (%)4.8
Misc. Trace Minerals (%)2.3
Nature of ResidueHigh Purity Quartz
Water of Plasticity (%)31
Wet Sieve Residue (%)0.34Wet Sieve Residue, +325 mesh
 0.39Wet Sieve Residue, +200 mesh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EOHC907 / 161986

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.