MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 30% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.46 - 1.60 g/cc0.0527 - 0.0578 lb/in³Average value: 1.51 g/cc Grade Count:10
Filler Content 30.0 %30.0 %Average value: 30.0 % Grade Count:3
Water Absorption 0.100 - 0.600 %0.100 - 0.600 %Average value: 0.303 % Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.00300 cm/cm0.00100 - 0.00300 in/inAverage value: 0.00219 cm/cm Grade Count:10
Linear Mold Shrinkage, Transverse 0.00450 - 0.00600 cm/cm0.00450 - 0.00600 in/inAverage value: 0.00528 cm/cm Grade Count:3
Melt Flow 5.50 - 30.0 g/10 min5.50 - 30.0 g/10 minAverage value: 11.3 g/10 min Grade Count:5
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 96.5 - 121 MPa14000 - 17500 psiAverage value: 112 MPa Grade Count:10
 52.0 - 125 MPa
@Temperature 0.000 - 160 °C
7540 - 18100 psi
@Temperature 32.0 - 320 °F
Average value: 91.5 MPa Grade Count:2
Elongation at Break 1.70 - 3.00 %1.70 - 3.00 %Average value: 2.17 % Grade Count:10
 1.60 - 1.80 %
@Temperature 60.0 - 150 °C
1.60 - 1.80 %
@Temperature 140 - 302 °F
Average value: 1.73 % Grade Count:1
Modulus of Elasticity 8.00 - 9.00 GPa1160 - 1310 ksiAverage value: 8.57 GPa Grade Count:9
 7.00 - 9.00 GPa
@Temperature 60.0 - 160 °C
1020 - 1310 ksi
@Temperature 140 - 320 °F
Average value: 7.94 GPa Grade Count:2
Flexural Yield Strength 145 - 185 MPa21000 - 26800 psiAverage value: 161 MPa Grade Count:8
Flexural Modulus 7.58 - 9.38 GPa1100 - 1360 ksiAverage value: 7.98 GPa Grade Count:8
Shear Modulus 0.0250 - 0.950 GPa
@Temperature 50.0 - 200 °C
3.63 - 138 ksi
@Temperature 122 - 392 °F
Average value: 0.669 GPa Grade Count:1
Izod Impact, Notched 0.641 - 0.961 J/cm1.20 - 1.80 ft-lb/inAverage value: 0.760 J/cm Grade Count:8
Izod Impact, Unnotched 3.74 - 5.87 J/cm7.00 - 11.0 ft-lb/inAverage value: 4.60 J/cm Grade Count:6
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²
@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 36.0 - 50.0 kJ/m²
@Temperature -25.0 - 120 °C
17.1 - 23.8 ft-lb/in²
@Temperature -13.0 - 248 °F
Average value: 41.3 kJ/m² Grade Count:1
Charpy Impact Unnotched 4.00 - 4.00 J/cm²
@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.00 J/cm² Grade Count:1
Charpy Impact, Notched 0.750 - 0.750 J/cm²
@Temperature -30.0 - -30.0 °C
3.57 - 3.57 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.750 J/cm² Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 2.00e+16 ohm-cm1.00e+12 - 2.00e+16 ohm-cmAverage value: 7.50e+15 ohm-cm Grade Count:4
Dielectric Constant 3.47 - 3.703.47 - 3.70Average value: 3.59 Grade Count:3
Dielectric Strength 16.9 - 45.0 kV/mm430 - 1140 kV/inAverage value: 27.0 kV/mm Grade Count:3
Dissipation Factor 0.000700 - 0.006000.000700 - 0.00600Average value: 0.00354 Grade Count:3
Comparative Tracking Index 125 - 250 V125 - 250 VAverage value: 161 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 - 22.0 µm/m-°C12.0 - 12.2 µin/in-°FAverage value: 21.7 µm/m-°C Grade Count:3
 25.0 - 25.0 µm/m-°C
@Temperature 140 - 180 °C
13.9 - 13.9 µin/in-°F
@Temperature 284 - 356 °F
Average value: 25.0 µm/m-°C Grade Count:1
Deflection Temperature at 0.46 MPa (66 psi) 187 - 190 °C369 - 374 °FAverage value: 188 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 166 - 260 °C331 - 500 °FAverage value: 194 °C Grade Count:10
Glass Transition Temp, Tg 187 - 265 °C369 - 509 °FAverage value: 232 °C Grade Count:3
Flammability, UL94 V-1 - 5VAV-1 - 5VAGrade Count:8
Oxygen Index 36.0 - 40.0 %36.0 - 40.0 %Average value: 38.0 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 271 - 410 °C520 - 770 °FAverage value: 354 °C Grade Count:10
Mold Temperature 93.3 - 210 °C200 - 410 °FAverage value: 152 °C Grade Count:9
Drying Temperature 110 - 191 °C230 - 376 °FAverage value: 148 °C Grade Count:9
Moisture Content 0.150 %0.150 %Average value: 0.150 % Grade Count:4
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:4
Injection Pressure 68.9 - 138 MPa10000 - 20000 psiAverage value: 101 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
Overview of materials for Polysulfone (PSU)
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 20%) Temper 25 mm rod
Overview of materials for Thermoset Fluoroelastomer

O5313 / 78484

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.