MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Sawbones Third-Generation Simulated Cortical Bone
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler; Filled/Reinforced Thermoset

Material Notes: E-glass-filled Epoxy

Sawbones® Third-Generation Bones model natural cortical bone using a mixture of short e-glass fibers and epoxy resin pressure injected around a foam core. The mid-shaft area has an intermedullarly canal.

Third-generation composite bone was developed to improve the composite bone physical behavior, increase anatomical detail in the cortical wall and ease manufacturing difficulties of the Second-Generation Bone.

Information provided by Sawbones.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 90.0 MPa13100 psi
Modulus of Elasticity 12.4 GPa1800 ksi
Compressive Yield Strength 120 MPa17400 psi
Compressive Modulus 7.60 GPa1100 ksi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sawbones Third-Generation Simulated Cancellous Bone (Solid)
Cortical Bone
Femur
Sawbones Third-Generation Simulated Cancellous Bone (Cellular)
Titanium Ti-6Al-4V (Grade 5), Annealed

PSAWBO00 / 66531

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.