MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Information provided by Dowell Trading Company Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 - 1.64 g/cc0.0571 - 0.0592 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.014 cm/cm0.0020 - 0.014 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9494ASTM D785
Tensile Strength, Ultimate 110 - 140 MPa16000 - 20300 psiASTM D638
Elongation at Break 4.0 - 5.0 %4.0 - 5.0 %ASTM D638
Flexural Yield Strength 150 - 230 MPa21800 - 33400 psiASTM D790
Flexural Modulus 7.00 - 10.0 GPa1020 - 1450 ksiASTM D790
Izod Impact, Notched 0.700 - 1.30 J/cm
@Thickness 6.35 mm
1.31 - 2.44 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
Dielectric Constant 3.5
@Frequency 60 Hz
3.5
@Frequency 60 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
584 kV/in
@Thickness 0.0787 in
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D150
Arc Resistance 100 sec100 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C
@Temperature 20.0 °C
16.7 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 225 °C437 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 208 °C406 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Chang Chun Plastic PBT2100 Fire Retardant PBT
Envalior Arnite® TV4 261 PBT-GF30, 30% Glass Filled
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler

PDOWELC39 / 30770

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.