MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAPAI™ CM XP403 PAI (Polyamide-imide), Unreinforced Stock Shapes
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Molded

Material Notes: Compression Molded

Main features:

  • good wear properties
  • excellent strength and stiffness
  • excellent dimensional stability
  • very good thermal stability
  • excellent chemical resistance
  • Target Industries:
    • electronics
    • aircraft and aerospace technology
    • oil and gas industry
    • chemical and refinery industry
    • process engineering

    Information provided by Ensinger

  • Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

    Click here to view all available suppliers for this material.

    Please click here if you are a supplier and would like information on how to add your listing to this material.

     
    Physical PropertiesMetricEnglishComments
    Density 1.41 g/cc0.0509 lb/in³
    Water Absorption 0.20 %
    @Time 86400 sec
    0.20 %
    @Time 24.0 hour
    ASTM D570
    Water Absorption at Saturation 1.7 %1.7 %ASTM D570
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore D 9090ASTM D2240
    Tensile Strength at Break 122 MPa17700 psiASTM D638
    Elongation at Break 6.4 %6.4 %ASTM D638
    Tensile Modulus 3.70 GPa537 ksiASTM D638
    Flexural Strength 145 MPa21000 psiASTM D790
    Flexural Modulus 3.91 GPa567 ksiASTM D790
    Compressive Strength  31.0 MPa
    @Strain 1 %
    4500 psi
    @Strain 1 %
    ASTM D695
     172 MPa
    @Strain 10 %
    25000 psi
    @Strain 10 %
    ASTM D695
    Compressive Modulus 2.58 GPa374 ksiASTM D695
    Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inASTM D256
    Limiting Pressure Velocity 0.350 MPa-m/sec10000 psi-ft/min100 fpm; safety factor = 4; ASTM D3702
     
    Electrical PropertiesMetricEnglishComments
    Surface Resistance 1.00e+13 ohm1.00e+13 ohmASTM D257
    Dielectric Constant 3.34
    @Frequency 1e+6 Hz
    3.34
    @Frequency 1e+6 Hz
    ASTM D150
    Dielectric Strength 13.7 kV/mm348 kV/inASTM D149
    Dissipation Factor 0.014
    @Frequency 1e+6 Hz
    0.014
    @Frequency 1e+6 Hz
    ASTM D150
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 38.7 µm/m-°C
    @Temperature -40.0 - 150 °C
    21.5 µin/in-°F
    @Temperature -40.0 - 302 °F
    ASTM E831
    Deflection Temperature at 1.8 MPa (264 psi) 257 °C494 °FASTM D648
    Glass Transition Temp, Tg 276 °C529 °FASTM D3418
    Flammability, UL94 V-0
    @Thickness 3.20 mm
    V-0
    @Thickness 0.126 in
     
    Descriptive Properties
    ColorGreen

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
    Syensqo (Solvay Specialty Polymers) Torlon® 4601 Polyamide-imide (PAI)
    Ensinger TECAPAI™ CM XP530 PAI (Polyamide-imide), Glass Fiber Filled Stock Shapes
    Ensinger TECAPAI™ CM XP440 PAI (Polyamide-imide), Graphite, PTFE Filled Stock Shapes
    EMS-Grivory Grilamid® TR 90 UV PAMACM12

    PENSIN893 / 239191

    Proto3000 – 3D Engineering Solutions

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.