MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.

Halar® is a trade name of Solvay Solexis, Inc. Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

New suppliers have been added for this product during the past 60 days.  

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ASTM D792
Water Absorption <= 0.10 %<= 0.10 %ASTM D570; 24 hrs.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.1 MPa4940 psiASTM D882
Elongation at Break 220 %220 %ASTM D882
Tensile Modulus 1.96 GPa284 ksiASTM D882
Flexural Modulus 1.65 GPa240 ksiASTM D790
Tear Strength 198 kN/m1130 pliASTM D1004
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
Dielectric Constant 2.56
@Frequency 1000 Hz
2.56
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 105 kV/mm
@Thickness 0.0762 mm
2670 kV/in
@Thickness 0.00300 in
ASTM D149
Dissipation Factor 0.0025 - 0.0050
@Frequency 1000 Hz
0.0025 - 0.0050
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 240 °C464 °FDSC
Maximum Service Temperature, Air 150 °C302 °FContinuous Use
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C145 °FASTM D648
Flammability, UL94 V-0V-0VTM-0
Oxygen Index 60 %60 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Halar® 500 ECTFE Fluoropolymer
Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Westlake Plastics Halar® 901 ECTFE
Syensqo (Solvay Specialty Polymers) Halar® 9414 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled
Syensqo (Solvay Specialty Polymers) Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled

PWEST086 / 72745

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.