Toppyl RC 3000 is an experimental fully formulated polyolefinic based easy peel/ reclosable solution. This product has been selected for use in peelable and reclosable seal to PE substrates (trays); used also in peelable and reclosable seal to APET. The material is readily processable on conventional blown and cast film equipment and is developed to be used as 100% in the easy peel layer of a co-extruded film structure. Toppyl RC 3000 provides an easy-opening and reclosable force over a wide sealing temperature window. Besides the easy-peel reclosable function, the material exhibit good optical properties and good organoleptic properties. Applications: Food Packaging Film, Peelable Film, Specialty FilmInformation provided by LyondellBasell. |