Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where electrostatic discharge behavior and good fuel resistance is required. Application examples: Connectors for fuel systems with antistatic properties. Information provided by EMS Grivory. |