MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
Categories: Polymer; Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 PF GC 201, DIN 7735 Hgw 2072, NF C26 150 GC, BS 3953 PF-2, NEMA LI 1 G-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.95 g/cc
@Temperature 23.0 °C
0.0704 lb/in³
@Temperature 73.4 °F
24h/23°C/50% RH; ISO 1183-A
Water Absorption 0.30 %0.30 %ISO 62-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 250 MPa
@Thickness >=1.50 mm
36300 psi
@Thickness >=0.0591 in
24h/23°C/50% RH; ISO 527
Flexural Strength 350 MPa
@Thickness >=1.50 mm
50800 psi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 19.0 GPa
@Thickness >=1.50 mm
2760 ksi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 500 MPa
@Thickness >=5.00 mm
72500 psi
@Thickness >=0.197 in
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 50.0 MPa
@Thickness >=5.00 mm
7250 psi
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 55.0 kJ/m²
@Thickness >=5.00 mm
26.2 ft-lb/in²
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+6 ohm1.00e+6 ohmafter immersion in water for 24 hr at 23°C
Dielectric Constant 5.0
@Thickness <=3.00 mm,
Frequency 50 Hz
5.0
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Dielectric Strength  1.18 kV/mm
@Thickness >=3.00 mm,
Temperature 90.0 °C
30.0 kV/in
@Thickness >=0.118 in,
Temperature 194 °F
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
 10.0 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
254 kV/in
@Thickness 0.118 in,
Temperature 194 °F
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
Dissipation Factor 0.030
@Thickness <=3.00 mm
0.030
@Thickness <=0.118 in
96h/105°C + 1h/23°C/20%RH; IEC 60250
Comparative Tracking Index 100 V
@Thickness >=3.00 mm
100 V
@Thickness >=0.118 in
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 155 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
311 °F
@Thickness >=0.118 in,
Time 20000 hour
IEC 60216
Flammability Test 5.0
@Thickness 3.00 mm
5.0
@Thickness 0.118 in
IEC 60695-11-10
 
Descriptive Properties
ColorDark brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Fabric Filled
G-3 Fiberglass Phenolic Laminate Sheet
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet
AISI 1340 Steel, normalized at 870°C (1600°F), air cooled, 25 mm (1 in.) round
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets

PELEKT043 / 126919

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.