MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos ABS Cadon® 127 SMA General Purpose, High Heat  (discontinued **)
Categories: Polymer; Thermoplastic; SMA Polymer; Styrene-Maleic Anhydride (SMA), Heat Resistant

Material Notes: Information provided by Bayer Corporation, Plastics Division

LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS. This product is no longer listed as a standard NAFTA product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 2.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104ASTM D785
Tensile Strength, Yield 34.0 MPa4930 psiASTM D638
Tensile Modulus 2.10 GPa305 ksiASTM D638
Flexural Yield Strength 66.0 MPa9570 psiASTM D790
Flexural Modulus 2.34 GPa339 ksiASTM D790
Izod Impact, Notched 1.00 J/cm
@Temperature -40.0 °C
1.87 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 2.10 J/cm
@Thickness 3.17 mm
3.93 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
@Thickness 13.0 mm
248 °F
@Thickness 0.512 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
@Thickness 13.0 mm
234 °F
@Thickness 0.512 in
ASTM D648
Vicat Softening Point 131 °C268 °FRate B; ASTM D1525
UL RTI, Electrical 100 °C
@Thickness 1.60 mm
212 °F
@Thickness 0.0630 in
UL746B
UL RTI, Mechanical with Impact 95.0 °C
@Thickness 1.60 mm
203 °F
@Thickness 0.0630 in
UL746B
UL RTI, Mechanical without Impact 95.0 °C
@Thickness 1.60 mm
203 °F
@Thickness 0.0630 in
UL746B
Flammability, UL94  HB
@Thickness 1.57 mm
HB
@Thickness 0.0618 in
 HB
@Thickness 1.57 mm
HB
@Thickness 0.0618 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Glass Reinforced, Modified SMA
Arkema OREVAC® 18910 Maleic Anhydride Modified Copolymer
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin
Dow Tyril® 100 SAN
Covestro Petlon® DP3-1039 Semi-Crystalline PET, 35% Glass Fiber

PB1C00 / 26409

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.