MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Insulcast® RTVS 27 HTC Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 27 HTC is a low viscosity, UL94V-0 certified, reversion resistant silicone compound. The combination of low viscosity and high thermal conductivity makes the RTVS 27 HTC ideal for potting dense component packages requiring heat dissipation.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.96 g/cc1.96 g/ccUncured. Part B
 1.98 g/cc1.98 g/ccUncured. Part A
Viscosity 3300 cP3300 cPPart B; ASTM D1084
 6000 cP6000 cPMixed, Part A, Part B; ASTM D1084
 8000 cP8000 cPPart A; ASTM D1084
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D2240
Tensile Strength 3.45 MPa500 psiASTM D412
Elongation at Break 60 %60 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.0075
@Frequency 1000 Hz
0.0075
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 170 µm/m-°C94.4 µin/in-°F
Thermal Conductivity 1.00 W/m-K6.94 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 120 °C
0.250 hour
@Temperature 248 °F
option
 30.0 min
@Temperature 95.0 °C
0.500 hour
@Temperature 203 °F
option
 120 min
@Temperature 60.0 °C
2.00 hour
@Temperature 140 °F
option
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
option
Pot Life 1.00 min1.00 minPart A, Part B
Shelf Life 6.00 Month6.00 MonthPart A, Part B
 
Descriptive Properties
ColorGraypart A, uncured
 Naturalpart B, uncured
Mix Ratio by volume1:1Part A: Part B
Mix Ratio by weight1:1Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives CoolTherm™ SC-252 Silicone encapsulant system
Lord Adhesives CoolTherm™ SC-104 Thermally Conductive Silicone Encapsulant
Lord Adhesives Circalok™ 6703A/B Thermally Conductive Two Part Silicone, Flame Retardant
ITW Insulcast® RTVS 3-95-2 Silicone Potting/Encapsulation Compound
ITW Insulcast® RTVS 3-95-1 Silicone Potting/Encapsulation Compound

PITWIN9118 / 239628

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.