MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Radici Radilon® A CP300K 333BK Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Mineral Filled

Material Notes: PA66 30% mineral filled, injection molding grade. Heat stabilized. Black color. Suitable for parts requiring good dimensional stability reduced shrinkage and low warp age.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³DAM; ISO 1183
Water Absorption 6.1 %
@Thickness 2.00 mm,
Temperature 23.0 °C
6.1 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Immersion; ISO 62
Moisture Absorption 1.90 %
@Thickness 2.00 mm,
Temperature 23.0 °C
1.90 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi5mm / min. Conditioned; ISO 527-2/1A
 90.0 MPa13100 psi5mm / min. DAM; ISO 527-2/1A
Elongation at Break 8.0 %8.0 %5mm / min. DAM; ISO 527-2/1A
 12 %12 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 4.20 GPa609 ksi1mm / min. Conditioned; ISO 527-2/1A
 5.20 GPa754 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 135 MPa19600 psi2mm / min. DAM; ISO 178
Flexural Modulus 4.50 GPa653 ksi2mm / min. DAM; ISO 178
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohm1.00e+12 ohmDAM; 500V.; IEC 60093
Comparative Tracking Index 500 V500 VDAM. Sol.A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75/2Af
Vicat Softening Point 245 °C
@Load 5.10 kg
473 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
0.000 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-1/2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6915 / 293420

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.