MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese VECTRA V140 LCP, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled

Material Notes: LCP/PPS blend. Maintains most of the characteristics of A130 with improved weldline strength. 40% glass reinforced.
VECTRA should in principle be predried. Because of the necessary low maximum residual moisture content the use of dry air dryers is recommended. The dew point should be =< - 40° C. The time between drying and processing should be as short as possible.
For subsequent storage of the material in the dryer until processed the temperature does not need to be lowered for grades A, B, C, D and V (<= 24 h).

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9696ISO 2039-2
Tensile Strength at Break 145 MPa21000 psi5mm/min; ISO 527-2/1A
Tensile Stress at Strain  20.83 MPa
@Strain 0.13 %,
Temperature 23.0 °C
3021 psi
@Strain 0.13 %,
Temperature 73.4 °F
 37.89 MPa
@Strain 0.27 %,
Temperature 23.0 °C
5495 psi
@Strain 0.27 %,
Temperature 73.4 °F
 55.06 MPa
@Strain 0.41 %,
Temperature 23.0 °C
7986 psi
@Strain 0.41 %,
Temperature 73.4 °F
 70.68 MPa
@Strain 0.55 %,
Temperature 23.0 °C
10250 psi
@Strain 0.55 %,
Temperature 73.4 °F
 85.36 MPa
@Strain 0.69 %,
Temperature 23.0 °C
12380 psi
@Strain 0.69 %,
Temperature 73.4 °F
 99.77 MPa
@Strain 0.82 %,
Temperature 23.0 °C
14470 psi
@Strain 0.82 %,
Temperature 73.4 °F
 113.19 MPa
@Strain 0.96 %,
Temperature 23.0 °C
16417 psi
@Strain 0.96 %,
Temperature 73.4 °F
 124.9 MPa
@Strain 1.1 %,
Temperature 23.0 °C
18120 psi
@Strain 1.1 %,
Temperature 73.4 °F
 135.82 MPa
@Strain 1.24 %,
Temperature 23.0 °C
19699 psi
@Strain 1.24 %,
Temperature 73.4 °F
 145.38 MPa
@Strain 1.38 %,
Temperature 23.0 °C
21086 psi
@Strain 1.38 %,
Temperature 73.4 °F
Elongation at Break 1.0 %1.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 16.0 GPa2320 ksi1mm/min; ISO 527-2/1A
Flexural Strength 230 MPa33400 psiISO 178
Flexural Modulus 16.0 GPa2320 ksiISO 178
Compressive Strength 134 MPa
@Strain 1 %
19400 psi
@Strain 1 %
ISO 604
Compressive Modulus 16.0 GPa2320 ksiISO 604
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243-1
Dissipation Factor  0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
IEC 60250
Arc Resistance 165 sec165 sec
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 11.0 µm/m-°C6.11 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 21.0 µm/m-°C11.7 µin/in-°FISO 11359-2
Melting Point 280 °C536 °FISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FISO 75-1, -2
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °Fhopper
 80.0 - 120 °C176 - 248 °Fcavity
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 295 - 305 °C563 - 581 °F
Zone 2 300 - 310 °C572 - 590 °F
Zone 3 300 - 310 °C572 - 590 °F
Zone 4 300 - 310 °C572 - 590 °F
Die Temperature 300 - 310 °C572 - 590 °F
Melt Temperature 293 °C559 °FISO 294
 300 - 315 °C572 - 599 °F
Mold Temperature 100 °C212 °FISO 294
Injection Velocity 150 mm/sec5.91 in/secISO 294
Drying Temperature 150 °C302 °F
Dry Time 4 - 24.0 hour4 - 24.0 hour
Moisture Content 0.010 %0.010 %Necessary low maximum
Injection Pressure 69.0 MPa10000 psiISO 294
 50.0 - 150.0 MPa7250 - 21750 psi
Hold Pressure 50.0 - 150.0 MPa7250 - 21750 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  80 rpm
@Diameter 40.0 mm
80 rpm
@Diameter 1.57 in
 140 rpm
@Diameter 25.0 mm
140 rpm
@Diameter 0.984 in
 200 rpm
@Diameter 16.0 mm
200 rpm
@Diameter 0.630 in
Hot-Working Temperature 300 - 310 °C572 - 590 °F
 
Descriptive Properties
Injection moldingYes
Injection speedvery fast
RemarksWhen using short metering strokes an accumulator is recommended to get short injection times

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott BG60 Bandpass Filter
Celanese Vectra® V140 Liquid Crystal Polymer (LCP), 40% Glass Reinforced
Celanese VECTRA S135 LCP, 35% Glass Reinforced
Schott IRG 24 Infrared Chalcogenide Glass

PHCS495 / 123910

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.